No | Properties | Units | Values | Remark |
1 | Composition | % | Y2O3+ZrO2≥99.5% | ZrO2≥95% |
2 | Density | g/cm³ | 5.95-6.05 | |
3 | Flexural Strength | Mpa | 800-1200 | |
4 | Tensile Strength | Mpa | 500-600 | |
5 | Weibull Modulus | M | >30 | |
6 | Compressive Strength | Mpa | >1950 | |
7 | Modulus of Elasticity | Gpa | 200 | |
8 | Poisson `s Ratio | 0.31 | ||
9 | Hardness | HV0.3kg/mm² | >1120 | HB≥87 |
10 | Fracture Toughness | Mpam¹/² | 8-10 | |
11 | Average Grain Size | μm | 0.4-0.6 | |
12 | Thermal Conductivity | W/m*K | 3.08 |
Element | C | Cr | Si | Mn | Mo | S、P |
Content | 2.8%-3.1% | 26%-28% | 0.6%-0.9% | 0.5%-1% | 0.5%-0.8% | <0.05% |
Plunger pump: SPM2250/2500, HT400, TWS 600, TWS 1000, OFM etc
Russian Pump: UNBT 950, UNB 600, 8T650 , UNBT 1180L, NBT 600, NBT 300 etc
Drillmec pump: 9T1000, 12T1600
Upetrom pump: 3PN1000 , 3PN1300/1600
Ellis Williams pump: E 447, E 2200
Omega: OPI 1000
BOMCO/Emsco/HongHua : FB1300/1600, F1300/1600, F800/1000, F500 & some Duplex pumps
G D : PZ 7, PZ 8/9, PZ 10/11, FK-FXK, FY-FXD, FD-FXX, FG-FXG, FQ-FXQ, FF-FXP , FG-GXG
National: 7P50, 8P80, 9P100, 10P130, 12P160, 14P220, JWS 165, JWS 340/400, C 250/350, K 700, K 500, K 380
Oilwell: A 560/600 PT, A 850/1100 PT, A 1400/1700 PT, 214P, 810P
Ideco: T 500, T 800/1000, T 1300/1600
Wirth: TPK1000, TPK1600, TPK 2000/2200
Weatherford: MP-5, MP-8, MP-10, MP-13, MP-16